Customization: | Available |
---|---|
Type: | Clay Dry Sand |
Casting Method: | Vacuum Aspirated Casting |
Still deciding? Get samples of US$ 0/Piece
Request Sample
|
Suppliers with verified business licenses
Audited by an independent third-party inspection agency
Product Specifications: |
|
Material: | Aluminum, A380, A356, ADC12, AlSi10Mg, 104, 102 etc. |
Dimension: | According to the drawing or sample |
Standard: | DIN GB ISO JIS BA ANSI |
Casting equipment: | 80T/160T/250T/300T/500Tcasting machine,Sand blasting machine,5T electri stove,Metallographic detector,Independent mould manufacturing |
Production Process: | Polish/Sand Blast/EDM/Milling/Texture/Grind/Pre-Treatment/Quenching/Lathe/Wire Cut/Annealing/Temper etc. |
Equipment of Casting: | 1. High pressure die casting machining:125T/180T/250T/280T/500T/800T/1250T 2. Gravity casting machine: 5 production lines 3. Low pressure die casting machining: 1 production line 4. Sand casting machine: 6 production lines 5. Degassing equipment and opportunities to refine the material 6. Machining: 5Sets CNC Machines;3 sets Milling machines; 3 setsTurning machines; 10 sets drill and tap machines |
Die component | Cast metal | |||||
Tin, lead & zinc | Aluminium & magnesium | Copper & brass | ||||
Material | Hardness | Material | Hardness | Material | Hardness | |
Cavity inserts | P20 | 290-330 HB | H13 | 42-48 HRC | DIN 1.2367 | 38-44 HRC |
H11 | 46-50 HRC | H11 | 42-48 HRC | H20, H21, H22 | 44-48 HRC | |
H13 | 46-50 HRC | |||||
Cores | H13 | 46-52 HRC | H13 | 44-48 HRC | DIN 1.2367 | 40-46 HRC |
DIN 1.2367 | 42-48 HRC | |||||
Core pins | H13 | 48-52 HRC | DIN 1.2367 prehard | 37-40 HRC | DIN 1.2367 prehard | 37-40 HRC |
Sprue parts | H13 | 48-52 HRC | H13 DIN 1.2367 |
46-48 HRC 44-46 HRC |
DIN 1.2367 | 42-46 HRC |
Nozzle | 420 | 40-44 HRC | H13 | 42-48 HRC | DIN 1.2367 H13 |
40-44 HRC 42-48 HRC |
Ejector pins | H13 | 46-50 HRC | H13 | 46-50 HRC | H13 | 46-50 HRC |
Plunger shot sleeve | H13 | 46-50 HRC | H13 DIN 1.2367 |
42-48 HRC 42-48 HRC |
DIN 1.2367 H13 |
42-46 HRC 42-46 HRC |
Holder block | 4140 prehard | ~300 HB | 4140 prehard | ~300 HB | 4140 prehard | ~300 HB |
The main disadvantage to die casting is the very high capital cost. Both the casting equipment required and the dies and related components are very costly, as compared to most other casting processes. Therefore, to make die casting an economic process, a large production volume is needed. Other disadvantages are that the process is limited to high-fluidity metals, and casting weights must be between 30 grams (1 oz) and 10 kg (20 lb).[note 3][10] In the standard die casting process the final casting will have a small amount of porosity. This prevents any heat treating or welding, because the heat causes the gas in the pores to expand, which causes micro-cracks inside the part and exfoliation of the surface.[4] Thus a related disadvantage of die casting is that it is only for parts in which softness is acceptable. Parts needing hardening (through hardening or case hardening) and tempering are not cast in dies.
Our advantage:
* One-Sotp service(from design to mass production)
* OEM /ODM Customized services
* Rapid prototyping & low-volume production
* High quality & low prices
* Highly skilled manufacturing process.
* Strict quality Control System.
Our promise:
* The delivery time and the package can be controled according to the customers' requirement completely.
* we will produce the products seriously according to the drawings, and make sure all the products is suitable for the custoners.
* We will communicate with the customers all the time about the products, we will send the pictures to the customers, so that they can know the Processing process
Our Policy:
Innovation and developing in Technique
High level of expertise
Outstanding quality
On-time delivery to customer needs
SERVICE: